This method is applicable to a concentration range of a mass fraction of -3,0 % to 7,0 % loss on ignition in natural iron ores, iron ore concentrates and agglomerates, and sinters.
The method is not applicable to the following:
- processed ores containing metallic iron (direct reduced iron);
- natural or processed ores in which the sulfur content is higher than a mass fraction of 0,2 %;
- internationally traded ores with combined water greater than 2,5 %.
NOTE 1 Loss on ignition can be used as an estimate of combined water.
NOTE 2 This method is intended for in-house use and is not intended for referee purposes.