1.1 This specification covers hot-worked alloy, carbon, and carbon-boron steels in a variety of compositions and sizes, which may attain specified depth of hardening in the end quench test. These steel compositions are identified by the suffix letter “H“ added to the conventional grade number.
1.2 This specification provides for analyses other than those listed under Tables 1 and 2. Special hardenability limits are also permissible when approved by the purchaser and manufacturer.
1.3 The values stated in inch-pound units are to be regarded as standard. No other units of measurement are included in this standard.
TABLE 2 Chemical Requirements of Carbon H-SteelsA
UNS DesignationB | Grade Designation | Chemical Composition, % | ||||
---|---|---|---|---|---|---|
Carbon | Manganese | Phosphorus, max |
Sulfur, max |
Silicon | ||
H 10380 | 1038 H | 0.34–0.43 | 0.50–1.00 | 0.040 | 0.050 | 0.15–0.35 |
H 10450 | 1045 H | 0.42–0.51 | 0.50–1.00 | 0.040 | 0.050 | 0.15–0.35 |
H 15220 | 1522 H | 0.17–0.25 | 1.00–1.50 | 0.040 | 0.050 | 0.15–0.35 |
H 15240 | 1524 H | 0.18–0.26 | 1.25–1.75 | 0.040 | 0.050 | 0.15–0.35 |
H 15260 | 1526 H† | 0.21–0.30 | 1.00–1.50 | 0.040 | 0.050 | 0.15–0.35 |
H 15410 | 1541 H | 0.35–0.45 | 1.25–1.75 | 0.040 | 0.050 | 0.15–0.35 |
H 15211C | 15B21 HC | 0.17–0.24 | 0.70–1.20 | 0.040 | 0.050 | 0.15–0.35 |
H 15351C | 15B35 HC | 0.31–0.39 | 0.70–1.20 | 0.040 | 0.050 | 0.15–0.35 |
H 15371C | 15B37 HC | 0.30–0.39 | 1.00–1.50 | 0.040 | 0.050 | 0.15–0.35 |
H 15411C | 15B41 HC | 0.35–0.45 | 1.25–1.75 | 0.040 | 0.050 | 0.15–0.35 |
H 15481C | 15B48 HC | 0.43–0.53 | 1.00–1.50 | 0.040 | 0.050 | 0.15–0.35 |
H 15621C | 15B62 HC | 0.54–0.67 | 1.00–1.50 | 0.040 | 0.050 | 0.40–0.60 |