1.1 This specification covers quenched-and-tempered carbon steel and high-strength low-alloy steel plates of structural quality for welded, riveted, or bolted construction.
1.2 If the steel is to be welded, it is presupposed that a welding procedure suitable for the grade of steel and intended use or service will be used.
1.3 Plates under this specification are available in four grades as follows:
Grade | Yield Strength, min, ksi [MPa] |
Tensile Strength, ksi [MPa] |
Maximum Thickness, in. [mm] |
A | 50 [345] | 70–90 [485–620] | 11/2 [40] |
B | 60 [415] | 80–100 [550–690] | 21/2 [65] |
C | A | A | 2 [50] |
D | 75 [515] | 90–110 [620–760] | 3 [75] |
A Varies with thickness. See Table 1.
1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system is to be used independently of the other.